Lancia Beta Forum
General Category => General Discussion => Topic started by: Duncan23 on May 04, 2011, 06:49:58 PM
-
I spoke to the steel stockist today about getting some sheet to make into my new floorpan (and offcuts to practise welding on). They asked whether I wanted pre-galv or CR4. What do you guys think I should use?
Pro galv:
increased protection when actually in the car
less rust while sat in the garage
No need to treat as soon as it's installed
Con:
slightly more expensive
care/cleaning needed when welding?
difficulty getting paint to stick
I don't thing it should be any harder to cut/shape than CR4. Maybe there would be fewer offcuts, but that doesn't really matter...
Have I missed anything? What's the consensus here?
Cheers
Duncan
-
Being in the metalwork game and having restored a few i would use zintec which is fully weldable, leaving good protection after welding. Cold reduced is prime quality but after welding the oil is burnt off allowing surface rust within hours.
-
I would ALWAYS go for the best material I can afford.
If it's rusted once it means that area is prone/susceptible. So even if it's a little more expensive to buy it protects your initial investment and the overall car.
Ask yourself this: Do you possibly want to re-visit the same area for a later repair because materials used in first repair are more prone to rusting?
-
I did some research and discovered zintec is significantly more convenient for welding and painting than pre-galv (you don't have to gind the coating off to weld it!). Unfortunately, the supplier didn't have zintec, but they can order it for me. So I got some CR4 off-cuts to practise welding/shaping with and I'll measure up and order zintec in the right sizes when I'm happy with my technique.
Thanks for the useful info. :)
Cheeers
Duncan
-
Duncan
What thickness are you using for your floorpans?
Rodders
-
I'm gonna try 1.6mm - if it's impossible to work and I want to put the grooves in I might go down to 1.2. Not decided how important the grooves are yet...